Decking timber in Australia is mostly hardwood, with H3 treated pine at the budget end. Six of the eight hardwoods compared below are rated Class 1 for durability above ground, which the Queensland Government puts at a life expectancy of more than 40 years3. So durability rarely decides it. Your Bushfire Attack Level narrows the list, the colour narrows it again, and what the deck drains onto matters because some timbers bleed more tannin than others. If nobody will clean and reseal the deck once a year, composite is the better fit.

Decking timber compared: durability, density, colour and bushfire rating

The table puts the common decking timbers side by side. Durability is the above-ground class of the heartwood, where Class 1 is the most durable. Density is air-dry, at 12% moisture content, with the Queensland Government's hardness rating on a 6-class scale3. The bushfire column is WoodSolutions' summary of AS 3959-2018 for the decking boards on a deck with an open subfloor11. The frame rules are in the next section.

TimberAbove-ground durabilityDensity and hardnessColourTannin bleedBushfire deckingIn the designer
Merbau (kwila)Class 1830 kg/m³, hard1Yellowish or orange-brown, darkening to brown or deep reddish-brownCan stain the work around it unless sealed on all sides, in WoodSolutions' note on merbau window joinery13Up to BAL-29Yes
Spotted gumClass 11,010 kg/m³, very hard2Light brown to dark red-brownLower than most other eucalypts13Up to BAL-29Yes
BlackbuttClass 1930 kg/m³, hard3Pale brown, faintly pink when freshly cutThe high extractives of mature wood can stain painted surfaces in the weather10Up to BAL-29Yes
Silvertop ashClass 2820 kg/m³, hard4Pale brown, sometimes pink-tingedNo species noteUp to BAL-29Yes
Grey boxClass 11,105 kg/m³, very hard5Pale brown, sometimes yellowishNo species noteBAL-12.5 and BAL-19Yes
JarrahClass 2835 kg/m³, hard6Dark redNo species noteBAL-12.5 and BAL-19, and BAL-29 in some circumstances12No
Grey ironbarkClass 11,105 kg/m³, very hard7Reddish brown to dark brownNo species noteBAL-12.5 and BAL-19No
TallowwoodClass 11,010 kg/m³, very hard8Pale to dark yellow-brownNo species noteBAL-12.5 and BAL-1912No
Treated pineTreated to H3; untreated radiata pine is Class 4545 kg/m³, soft9Untreated sapwood pale yellow to whiteCan bleed resin12No BAL listed12No

Where the tannin column says no species note, none of the sources cited here gives one for that timber, which doesn't mean it is free of tannin. WoodSolutions' deck guide says most hardwoods carry water-soluble extractives that leach to the surface as the timber dries, and the stain can be hard to remove from unsealed brick, concrete or paving under the deck12.

The ironbark row is grey ironbark, the timber the Queensland Government page describes. Red ironbark, also sold as decking, is Class 1 above ground and a bushfire-resisting timber for decking up to BAL-29 in WoodSolutions' deck guide12. Silvertop ash is the one to read twice. It is on the bushfire list, but it is also Class 3 in the ground and not termite resistant, according to the Queensland Government4.

Which timber is best for decking?

The right timber is the one that suits your bushfire level, what the deck drains onto and the colour you want, because durability is similar across most of the table.

On a bushfire-prone block, the BAL narrows the list first. WoodSolutions names seven bushfire-resisting timbers: blackbutt, kwila (merbau), red ironbark, river red gum, silvertop ash, spotted gum and turpentine11. They can be decking up to BAL-29. Grey box and grey ironbark are on a second list with jarrah, for species with a density of 750 kg/m³ or more11. That list covers decking at BAL-12.5 and BAL-19.

The frame rules depend on the subfloor. At BAL-29 an open subfloor needs bushfire-resisting timber for the supports and framing as well as the boards. With an enclosed subfloor the summary lets you build the supports and framing as usual. At BAL-40 and BAL-FZ it points to alternatives to timber for the decking, and for the whole deck when the subfloor is open11.

If the deck drains onto pale paving, a pool surround or a light wall, tannin matters more than hardness. WoodSolutions' finishing guide gives spotted gum a lower tannin content than most other eucalypts, so its run-off is less likely to stain paintwork and brickwork13. Merbau is the one I'd keep away from pale surfaces, and the merbau decking guide shows why.

Colour is the last cut. For a pale deck the table points to blackbutt, tallowwood or grey box. Jarrah and merbau give the red end.

A deck less than 400 mm off the ground needs more ventilation and drainage under it, and more durable or treated timber, according to WoodSolutions' deck design guide12. I'd stick to the Class 1 timbers there.

Hardwood decking: the common species in brief

Merbau

Merbau, also sold as kwila, is the imported one. It is a tropical hardwood whose heartwood is yellowish or orange-brown when cut and turns brown or deep reddish-brown with age1. I'd coat every face before it goes down and ask for certified stock.

Spotted gum

Spotted gum is the one timber in the table with a low-tannin note as well as Class 1 durability and a place on the bushfire-resisting list. It is very hard, and gum veins are common in it. Read the spotted gum decking guide for the oiling.

Blackbutt

Blackbutt gives a pale deck that is Class 1 above ground and on the bushfire-resisting list. Its extractives can stain paint, so I'd oil it rather than paint it.

Silvertop ash

Silvertop ash is pale brown with occasional gum veins and flecks4. It is on the bushfire-resisting list, which is its main draw, and it is the least durable hardwood in the designer.

Grey box

Grey box is the densest timber in the designer, and it is Class 1 in the ground as well as above it5. It isn't on the bushfire-resisting list, so on a bush block it covers decking at BAL-12.5 and BAL-19 only.

Jarrah

Jarrah grows only in the south-west of Western Australia, and the heartwood is dark red6. It is Class 2 above ground and isn't in the designer.

Ironbark

Grey ironbark is among the hardest and heaviest timbers in the table. One owner on Whirlpool, GQV1750, chose ironbark for a renovation about eight years before writing in September 2015: "We ended up with ironbark which has hardly weathered if at all"15. Ask which ironbark is in the pack, because red and grey sit on different bushfire lists.

Tallowwood

Tallowwood's heartwood is pale to dark yellow-brown and usually free from gum veins8. It is Class 1 above and in the ground. It is a good pale alternative where the BAL is 19 or lower.

Where does treated pine fit?

Treated pine is the softwood option, treated to H3 for decks. Untreated radiata pine is Class 4 and soft, rated 5 on the 6-class scale9. The treatment is what makes it last outdoors. It needs closer joists too. AS 1684 allows 450 mm centres under 22 mm treated softwood decking, against 500 mm under 19 mm hardwood12. It isn't on the bushfire lists for decking, and the treated pine decking guide covers the grades, the finish and the safety points.

Timber decking prices: what changes the cost

I don't print timber prices, because they change too often and each species comes in grades, widths and lengths that are priced separately. These are the things that move a quote.

Species is the obvious one, though owners don't always find a big gap. In a September 2015 Whirlpool thread weighing merbau against Australian hardwood, The M575, who built in spotted gum, wrote: "Price difference was not much"15.

Grade matters too. Hardwood decking is sold to an appearance grade, and Select carries fewer features than Standard or Medium Feature grade12. Get the grade written on every quote.

Seasoning is the hidden one. Unseasoned boards are laid tighter, at 2–3 mm, because they shrink, while seasoned hardwood 86–90 mm wide goes down at 3–4 mm12. Pharma.., who has bought tallowwood direct from a mill on the New South Wales mid north coast, warned in August 2022 that such boards may not be kiln dried, and described what happened to theirs: "I laid them spaced 4mm and 5 years later had some gaps over 10mm"16. A pack that isn't kiln dried can cost you later, in gaps.

Then count the upkeep. WoodSolutions' deck guide says a timber deck should be cleaned and resealed or stained at least once a year, or as the coating maker says12. Put those days and that coating in any comparison with composite.

When is composite the better choice?

When the deck won't get its yearly clean and coat. One composite maker says its boards don't need oiling, sanding or painting14. Owners split on whether the oiling is a burden. In an August 2022 Whirlpool thread, outoftheknow wrote: "I give my two Merbau decks a clean and coat once per year when I can be bothered"16. In the same thread WhoMastadon, defending composite, said theirs had been mopped with water maybe twice in six years and "looks as good as when it was installed"16.

Composite also fits two other cases. One is a bush block at BAL-40, where WoodSolutions' summary points to alternatives to timber11. One composite brand states a rating to that level, as composite decking fire ratings explains. The other is a deck over pale paving or a pool surround, where you don't want hardwood tannin running onto it.

Timber keeps two advantages. The same maker says its composite boards get hotter than timber in direct sunlight, and can't be sanded back the way timber can14. On a west-facing deck used barefoot, I'd stay with a pale timber or choose a light composite colour. The composite decking hub lists each range with its price for your state.

What I'd do

If the block is bushfire-prone, get the BAL assessment before choosing anything, because it sets the list of species and the frame. Then look at where the deck's water goes. Over pale paving, choose spotted gum or plan to seal the paving first. Pick the colour from what's left, and ask for kiln-dried boards with the grade written on the quote. Decide now whether you'll clean and reseal every year. If you won't, price composite on the same drawing. The deck designer has five of these hardwoods as well as composite ranges, so you can draw your deck in each and compare what it needs.